Alloy HX is a nickel-iron chromium alloy with good high-temperature strength and corrosion resistance. It provides good resistance to oxidation and carburization.
Typical applications: heat-treating equipment, industrial furnaces, and nuclear engineering.
Typical Chemical Composition % (max values, unless noted) | |||||||
---|---|---|---|---|---|---|---|
Nickel | Remainder | ||||||
Chromium | 20.5-23.0 | ||||||
Iron | 17.0-20.0 | ||||||
Molybdenum | 8.0-10.0 | ||||||
Cobalt | .5-2.5 | ||||||
Sulfur | 0.03 | ||||||
Tungsten | .2-1.0 | ||||||
Carbon | .05-0.15 | ||||||
Manganese max | 1.0 | ||||||
Silicon max | 1.0 | ||||||
Phosphorous max | 0.04 |
Typical Mechanical Properties | |||||
---|---|---|---|---|---|
Annealed | ksi | Mpa | |||
Yield Strength (0.2% offset) | 55-62 | 379-427 | |||
Tensile Strength | 117-122 | 807-841 | |||
Elongation % | 44-48 |